The CLR-HP is good for up to about 200 deg.F. with a structural load. After 200 deg. it will begin to flex. Watch for yellowing of the epoxy as a sign of heat stress, as you cycle the piece. I think you will be ok....with perhaps a little stress around the mount's ...where the metal screws connects the heat transfer to the pipe. Generally speaking, when I use any parts for muffler I use 1618, as it is good up to 250 deg.F......or in the case of header heat shields.....Max-hte.....
I have no clue how hot the dr's muffler get's.... But just be on the look out when you make parts for exhausts systems....